Salt Bath QPQ Treatment Optimizes Wear and Corrosion Resistance in 42CrMo4
A research collaboration across Chinese academic and industrial engineering institutes has demonstrated that liquid Quench-Polish-Quench, or QPQ, surface modification can simultaneously optimize the surface microhardness, sliding wear performance, and electroc
Illustrative imageA research collaboration across Chinese academic and industrial engineering institutes has demonstrated that liquid Quench-Polish-Quench, or QPQ, surface modification can simultaneously optimize the surface microhardness, sliding wear performance, and electrochemical corrosion resistance of 42CrMo4 alloy steel. Reporting in Frontiers in Materials, the investigators systematically tracked how adjusting salt-bath nitrocarburizing temperatures between 560 degrees Celsius and 580 degrees Celsius and holding times between 1.5 hours and 2.5 hours controls microstructural growth and phase composition. Their experimental evaluations identify a nitrocarburizing stage held at 570 degrees Celsius for 2.0 hours as the optimal processing window, establishing a dense surface compound layer paired with a continuous nitrogen diffusion zone that achieves an exceptional balance between high surface hardness and core toughness.
Gears manufactured from alloy steels are critical transmission components in heavy-duty machinery such as coal mining shearers, where components must endure severe dynamic impact loads, intense surface abrasion, and demanding fatigue conditions. While 42CrMo4 steel is frequently selected for these mechanical assemblies because of its strong hardenability, baseline toughness, and low quenching distortion, metallic gear failures routinely originate at component surfaces from defects or crystallographic slip deformation. Mainstream commercial hardening methods exhibit notable engineering disadvantages: high-temperature gas carburizing induces significant thermal distortion, high operating expenses, and susceptibility to case spalling, whereas conventional gas nitriding involves extended processing cycles, high surface brittleness, and inconsistent case depth. Liquid salt-bath QPQ processing provides an environmentally sound alternative that introduces nitrides, carbides, and protective oxides into the near-surface lattice with minimal workpiece distortion.
To evaluate these surface evolutions under controlled laboratory settings, normalized 42CrMo4 steel specimens containing 0.45 percent carbon, 1.2 percent chromium, 0.8 percent manganese, 0.37 percent silicon, and 0.25 percent molybdenum were machined and oil-quenched from 860 degrees Celsius before being tempered at 420 degrees Celsius. The steel blocks were then subjected to salt-bath nitrocarburizing at designated operating temperatures in a nitriding furnace with a cyanate ion concentration of 33 percent, followed by controlled post-oxidation in an oxidation furnace. Cross-sectional microstructures, elemental profiles, and phase constituents were characterized using metallurgical optical microscopy, field-emission scanning electron microscopy equipped with energy-dispersive X-ray spectroscopy, and X-ray diffraction running Cu radiation from 20 degrees to 100 degrees at two degrees per minute.
Microstructural analyses revealed that salt-bath nitrocarburizing constructs a characteristic layered architecture consisting of an outermost iron oxide film, an intermediate white compound layer, and an underlying nitrogen diffusion zone extending into the steel substrate. Across all examined parameters, the primary strengthening constituents identified by X-ray diffraction patterns were hard zeta-Fe2N iron nitrides, an Fe3O4 magnetite oxide film, and smaller proportions of epsilon-Fe3N. Increasing nitrocarburizing temperature accelerated the diffusion activation energy and atomic migration rate of active nitrogen, progressively intensifying the characteristic diffraction peaks of zeta-Fe2N. The accompanying post-oxidation step generated a continuous Fe3O4 film that filled microscopic voids within the porous outer nitride sublayer, sealing the surface against aggressive chemical species and mitigating metal-to-metal contact during mechanical sliding.
When assessing nitrocarburizing holding durations of 1.5, 2.0, and 2.5 hours at a constant temperature of 560 degrees Celsius, the team observed that surface microhardness and effective case depth initially increased rapidly before reaching a dynamic saturation plateau. A brief 1.5-hour treatment produced an insufficient surface hardness of 766.3 HV0.3 and a shallow, abrupt transition zone due to limited atomic migration. Extending holding duration to 2.0 hours elevated surface microhardness to 824.2 HV0.3 and smoothed the transition into the 340 to 360 HV0.3 substrate. Tribological ball-on-disc dry sliding tests performed against silicon nitride balls under a 10-Newton normal load demonstrated that the average friction coefficient dropped from 0.56 at 1.5 hours to 0.38 at 2.0 hours, while cumulative wear mass loss fell from 2.61 milligrams to 0.49 milligrams. However, prolonging holding to 2.5 hours produced embrittlement, increasing mass loss to 1.70 milligrams.
Treatments evaluated across holding times at 570 degrees Celsius yielded superior microstructural density and tribological response compared to identical durations at lower temperatures. After 1.5 hours at 570 degrees Celsius, specimens exhibited steep hardness gradients, producing an average friction coefficient of 0.43 and a wear mass loss of 0.91 milligrams characterized by microcracking under contact shear. Holding the specimens for 2.0 hours at 570 degrees Celsius delivered the best overall mechanical profile: surface microhardness peaked at 892.6 HV0.3, the cross-sectional hardness decline was continuous, the average friction coefficient dropped to 0.29, and sliding mass loss reached a study low of 0.19 milligrams. Extending the process to 2.5 hours degraded case cohesion, as dispersed acicular and granular nitrides coarsened into blocky carbonitrides, causing localized microspalling that elevated wear mass loss back to 0.32 milligrams.
Elevating the salt-bath temperature to 580 degrees Celsius further stimulated solid-solution and precipitation reactions, but introduced structural defects associated with thermal overexposure. Although a 2.0-hour dwell at 580 degrees Celsius yielded the highest absolute surface microhardness at 902.4 HV0.3, extended holding for 2.5 hours triggered local porosity, microvoid growth, and nitride coarsening that compromised interfacial bonding and caused the hardness to decline to 876.2 HV0.3. Friction and wear testing at 580 degrees Celsius reflected this brittleness: while the 2.0-hour specimen exhibited a friction coefficient of 0.28 with 0.62 milligrams of wear loss, the 2.5-hour specimen suffered severe abrasive and adhesive wear, generating loose debris that acted as third-body abrasives, causing wear loss to reach 0.59 milligrams alongside large friction fluctuations.
A direct tribological comparison among specimens treated for 2.0 hours across the three temperatures underscored the mechanical supremacy of the 570 degrees Celsius condition under room-temperature dry sliding. The 560 degrees Celsius specimen demonstrated unstable frictional behavior, exhibiting an average friction coefficient of roughly 0.38 alongside elevated wear. While the 580 degrees Celsius specimen achieved a comparable friction coefficient of 0.28, its wear rate of 1.5 multiplied by 10 to the negative seventh grams per Newton-meter was notably higher than that of the 570 degrees Celsius sample, which achieved an optimal wear rate of only 1.0 multiplied by 10 to the negative seventh grams per Newton-meter. Scanning electron microscopy confirmed that the 570 degrees Celsius surface suppressed microcutting and adhesive gouging through its smooth, intact Fe3O4 lubricating film backed by a rigid nitride sublayer.
Potentiodynamic polarization and electrochemical impedance spectroscopy carried out in 3.5 weight percent sodium chloride solutions demonstrated pronounced temperature-dependent corrosion resistance. The specimen modified at 570 degrees Celsius for 2.0 hours demonstrated a corrosion current density of approximately 1.1 multiplied by 10 to the negative fifth amperes per square centimeter, which was one order of magnitude lower than the 560 degrees Celsius sample at 1.2 multiplied by 10 to the negative fourth amperes per square centimeter and two orders of magnitude lower than the 580 degrees Celsius sample at 1.3 multiplied by 10 to the negative third amperes per square centimeter. Furthermore, the 570 degrees Celsius specimen maintained an expansive, stable anodic passive range extending between minus 0.5 volts and 0 volts, signifying the formation of an unruptured electrochemical barrier.
Microscopic energy-dispersive X-ray mapping of surfaces following electrochemical exposure provided structural verification for these distinct corrosion behaviors. On specimens treated at 560 degrees Celsius, discontinuous oxide formation and insufficient chromium diffusion permitted electrolyte ingress, resulting in widespread substrate dissolution, microcracking, and localized iron depletion. At 580 degrees Celsius, severe elemental segregation, coarse nitrides, and microstructural defects generated porous, non-protective iron oxide clusters that fostered deep pitting attack. In sharp contrast, the 570 degrees Celsius treated case exhibited exceptionally uniform, continuous spatial distributions of iron, nitrogen, and chromium without localized elemental clustering or depletion, confirming that an optimal thermal balance produces an integrated, defect-free composite shield against corrosive media.
The study clarifies that the strengthening mechanism of QPQ-treated 42CrMo4 steel does not stem from singular surface phase hardening, but from the coordinated synergy of a load-bearing zeta-Fe2N compound layer, a smoothly graded nitrogen diffusion zone, and a dense, self-lubricating Fe3O4 outer film. The investigators noted that their single-factor experimental design held cyanate concentration, pre-treatment steps, and oxidation parameters constant, precluding full statistical decoupling of complex variable interactions. Consequently, the authors suggest implementing response surface methodology in future studies to model the coupled kinetics of holding time and bath temperature, while providing practical technical validation for applying optimized 42CrMo4 surface treatments to high-load mining machinery gear transmissions.
Subject of Research: Microstructural evolution, tribological behavior, and corrosion resistance of 42CrMo4 steel subjected to quench-polish-quench surface treatment.
Article Title: Effect of QPQ treatment on microstructure and properties of 42CrMo4 steel
Article References: Ma, Y., Yuan, H., Zhang, S., Chen, C., Li, F., Yuan, R., Huang, Q., Liu, C., & Qiu, J. (2026). Effect of QPQ treatment on microstructure and properties of 42CrMo4 steel. Frontiers in Materials, 13, Article 2035194. https://doi.org/10.3389/fmats.2026.2035194
Image Credits: AI Generated
DOI: 10.3389/fmats.2026.2035194
Keywords: 42CrMo4 steel, QPQ treatment, salt bath nitrocarburizing, wear resistance, corrosion resistance, surface modification, microstructure, microhardness, friction coefficient, compound layer, diffusion layer, iron nitrides, Fe3O4 oxide film, polarization curves, electrochemical corrosion, mining machinery gears, X-ray diffraction